Mass fraction of nickel, wt%, not higher than | 54 |
Mass fraction of sulfide sulfur, wt%, not higher than | 0.38 |
Activity (according to technical specifications) as determined in the hydrogenation of pseudocumene, %, not less than | 65 |
Selectivity determined in the hydrogenation of acetylene, %, not less than | 73 |
Bulk density, g/cm3, not less than | 1.15 |
Crushing force applied to the element of cylinder, kg/tablet average, not less than minimum, not less than | 8.0 5.0 |